英语翻译制备接枝环氧树脂时,BPO最佳用量为占环氧用量的3%,环氧占共聚物最佳用量24%,丙烯酸占单体最佳用量19%;制
英语翻译
制备接枝环氧树脂时,BPO最佳用量为占环氧用量的3%,环氧占共聚物最佳用量24%,丙烯酸占单体最佳用量19%;制备接枝环氧乳液时,各种试剂最佳配比为接枝环氧:乳化剂:溶剂:水=1:0.1:0.5:2;制备复合乳液时,接枝环氧乳液与苯丙乳液复配最佳比例为2:8,涂膜表干时间16min,外观性能优良,涂膜硬度3H,耐水性260min,附着力1级
when preparing graft epoxy,the optimum amount of BPO accounts for 3% of the epoxy,epoxy accounts for 24% of copolymer,acrylic accounts for 19% of monomer mixture; when preparing graft epoxy emulsion,the optimal ratio of graft epoxy,emulsifier,solvent and water is 1:0.1:0.5:2; when preparing the composite latex,the best ratio of graft epoxy emulsion and styrene-acrylic emulsion is 2:8,the dry time is 16min,appearance is excellent,film hardness is 3H,water resistance is 260min,adhesion is 1